ks65609
Member
- Aug 30, 2009
- 342
- Boat Info
- 1992 330 Sundancer
- Engines
- Twin 454 Mercruiser--340hp
V drive inboards
We have always used vc17 bottom paint and always in fresh water. In the same marina for years. This year's haul out presented us with some type of blistering or apparent damage to the bottom paint in the areas of the trim tabs and centre anode. All anodes were replaced this year with magnesium. We have never had any issue such as this. The marina as well is in the process of trying to figure out what may have occured. Our slip neighbours do not have any type of similar situation. I would sure appreciate any input or feedback from anyone with experience in this area. We spend considerable time and effort trying to keep our boat in top condition and find this very disturbing. There is no apparent damage to the gel coat.
Thanks very much
Ken
http://s1091.photobucket.com/user/ks65609/slideshow/92 330 sundancer
http://s1091.photobucket.com/user/ks65609/media/92 330 sundancer/IMG_1935.jpg.html?sort=3&o=1
Thanks very much
Ken
http://s1091.photobucket.com/user/ks65609/slideshow/92 330 sundancer
http://s1091.photobucket.com/user/ks65609/media/92 330 sundancer/IMG_1935.jpg.html?sort=3&o=1