Looking for advice, recommendation, etc for a good fairing compound for below the waterline use. I have a few gelcoat blisters that I am going to address this winter while my boat is on the hard. The blisters have been "popped" and are drying. Next step is to sand/grind the edges back in preparation for fairing.
The blisters are located near the aft transduecer location. This area is covered with bottom paint. I do NOT intend to put gelcoat over the repair. Would I need to put an epoxy barrier coat over the fairing compound? Are any primers needed before application of anti-foul paint?
The total area is going to be less the 1 square foot.....much less actually.
Any advice or guidance is appreciated.
Jaybeaux
The blisters are located near the aft transduecer location. This area is covered with bottom paint. I do NOT intend to put gelcoat over the repair. Would I need to put an epoxy barrier coat over the fairing compound? Are any primers needed before application of anti-foul paint?
The total area is going to be less the 1 square foot.....much less actually.
Any advice or guidance is appreciated.